本站大部份資料在 2016 年後就未更新,若資料內無明確標示資料時間,請預設該資料為過時資料並斟酌使用,謝謝
column | value |
---|---|
Title | 天然皮革廢料回收再生製程技術 |
Abstract | 將回收之皮革以抓式粉碎法製成皮纖維後利用乳膠(NR/SBR=4:6)進行纖維補強可得到較佳之物性強度。在操作製程研究中發現游離度在680-760/3g、皮漿濃度2%、pH=8.2、溫度在80℃時可得到較佳之操作穩定性及產品物性。 |
EngTitle | Applied Technology in Recycling Leather Board Production. |
EngAbstract | Using the latex solution,the ratio of NR/SBR = 4:6 is the best formula ,as a reinforcement agent to improve the physical strength of leather board, which was made of recovery leather fiber.In the process of leather board producing, the physical properties of the product and the operating system would be better under the following operating conditions: the concentration of leather fiber:2%;pH=8.2;temp.=80℃;degree of freedom=680-760/g. |
ProjectYear | 094 |
SponsorOrg | 永續發展室 |
ExecutingOrg | 財團法人鞋類暨運動休閒科技研發中心 |
PublicFullVersionURL | http://epq.epa.gov.tw/project/FileDownload.aspx?fid=4390 |